Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CP PRYME® Polycarbonate PC100RUL-18M BT Clear - PC - Chase Plastics

Material Data Center offers the following functions for CP PRYME® Polycarbonate PC100RUL-18M BT Clear:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other CP Pryme datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Índice de fluidez, MFI 18 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Contracción posterior al moldeo, paralelo 0.006 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 65 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 11 kJ/m² ISO 179/1eA
Resistencia al impacto Izod, +23°C N kJ/m² ISO 180/1U
Resistencia al impacto Izod con entalla, +23°C 65 kJ/m² ISO 180/1A
ASTM Data
Esfuerzo de fluencia a tracción 62.1 MPa ASTM D 638
Esfuerzo de fractura a tracción 68.9 MPa ASTM D 638
Alargamiento a la fluencia 7 % ASTM D 638
Alargamiento a la rotura 130 % ASTM D 638
Módulo de flexión 2340 MPa ASTM D 790
Dureza Rockwell R118 - ASTM D 785
Resistencia a la abrasión (Taber) 10 mg/1000 cycles ASTM D 1044
Resistencia al impacto Izod con entalla, 1/8 in 690 J/m ASTM D 256
Resistencia al impacto Izod, 1/8 in 3200 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Combustibilidad UL 94 HB - UL 94
Estabilidad al calor @ 66 psi 138 °C ASTM D 648
Estabilidad al calor @ 264 psi 129 °C ASTM D 648
Temperatura Vicat 154 °C ASTM D 1525
Conductividad térmica, estado sólido 0.036 W/(m K) ASTM C 177
Calor específico 1260 J/(kg K) ASTM C 351
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Opacidad 1 % ASTM D 1003
Transmitancia luminosa 88 % ASTM D 1003
Índice de refracción 1.59 - ASTM D 542
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua, 24hr 0.15 % ASTM D 570
Absorción de agua, equilibrio 0.35 % ASTM D 570
Densidad 1200 kg/m³ ASTM D 792
Características
Forma de suministro
Sémola
Características especiales
Transparente
Disponibilidad regional
Norteamérica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.